Loading

Evaluation of Physical Properties of Silica filled Resin Based Dental Composites
Bhanu Pratap1, Ravi Kant Gupta2
1Bhanu Pratap, Department of Mechanical Engineering, Manipal University Jaipur, Rajasthan, India-303007
2Ravi Kant Gupta, Department of Mechanical Engineering, Manipal University Jaipur, Rajasthan, India-303007 
Manuscript received on February 05, 2019. | Revised Manuscript received on February 14 2019. | Manuscript published on August 30, 2019. | PP: 5047-5049 | Volume-8 Issue-6, August 2019. | Retrieval Number: F9548088619/2019©BEIESP | DOI: 10.35940/ijeat.F9548.088619
Open Access | Ethics and Policies | Cite | Mendeley
© The Authors. Blue Eyes Intelligence Engineering and Sciences Publication (BEIESP). This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)

Abstract: In this study, resin based dental composites were developed using monomers Bis GMA and TEGDMA, CQT and DMAEA. Silica were filled as filler material. After curing, the samples were tested for void content and water sorption and solubility. The results showed that as the void content increases, water sorption also increases in resin based dental composites. In brief, it can be stated through this experimental study that with the increase in silica filler upto 9 %wt, void content and water sorption both increases.
Keywords: Dental Composites, Resin etc.